Observation Examples of Polymers
Observation of Lamellar Structure of Polyethylene Film
![Observation of Lamellar Structure of Polyethylene Film](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn50420000007361-img/qn5042000000736i.jpg)
Surface observation of polyethylene film was performed to simultaneously obtain a 3D image and a Viscoelastic image. In the Viscoelastic image on the right, the lamellar structure can be observed; crystallization is more advanced in whiter parts, which are harder. Each image covers an area of 1 µm x 1 µm.