Observation Examples of Living Organisms

Observation of Cellulose

Observation of Cellulose

This image shows the cellulose fibers in nata de coco and the Acetobacter xylinum that creates them. It can be seen clearly how the fibers, which are only a few tens of nanometers thick, cross over each other.