Observation Examples of Polymers
Example of the observation of a dispersing agent
![Example of the observation of a dispersing agent](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000073do-img/qn504200000073e5.jpg)
The dispersion pattern of a dispersing agent was observed in a polymeric material. In the surface potential image (right), potential differences are observed as a result of differences in material, creating an image of solid-state property differences other than surface form (left). (Q control system application)