Observation Examples of Polymers
Observation of Laminated Plastic
![Observation of Laminated Plastic](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000073i9-img/qn504200000073iq.jpg)
Topographic Image (above) & LFM Image (below)
The sample is grasped by the holder, a cross section produced, and observed. With the LFM image the cross section layer structure appears from large and small friction forces caused by the difference in molecular weights.