Observation Examples of Nanotechnology
Gold Ultrathin Nanowires
![](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/n9j25k00000nc4ht-img/n9j25k00000nc4sb.jpg)
![](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/n9j25k00000nc4ht-img/n9j25k00000nc4nv.jpg)
Gold Ultrathin Nanowires were observed in air. Nanowires are a new material that is expected to be applied in areas such as pressure sensors and nanocoils.
The structure of the nanowires supported on a substrate was observed (Figs. 1 and 2), as was a bundle structure formed by a number of nanowires (Fig. 3).
The image in Fig. 3 is a superposition of height and phase images, which clearly shows the bundle structure of nanowires.
Samples Provided By: Dr. Yamazoe, Tsukuda Laboratory, School of Science, the University of Tokyo
References: Ryo Takahata, et al.,J. Am. Chem. Soc.2014, 136, 8489-8491.