Observation Examples of Polymers
Humidity-Controlled Observations and Force Curve Measurements of a Nafion® Film
Changes in the shape of the surface of a Nafion® film due to changes in humidity were observed at humidity values between 10 and 80 %. It was evident that the film expanded due to moisture absorption.
![Humidity-Controlled Observations and Force Curve Measurements of a Nafion® Film](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/
an/n9j25k00000deksd-img/n9j25k00000dekxt.jpg)
After the probe had made contact with the sample surface, it was gradually separated from the sample. At this point, a force curve measurement was also performed by measuring the force acting between the probe and sample.
![Humidity-Controlled Observations and Force Curve Measurements of a Nafion® Film](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/
an/n9j25k00000deksd-img/n9j25k00000dekxl.jpg)
The adhesion force increased rapidly when the humidity changed from 40 to 50 %.
![Humidity-Controlled Observations and Force Curve Measurements of a Nafion® Film](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/
an/n9j25k00000deksd-img/n9j25k00000dekxd.jpg)