Observation Examples of Polymers
Dewetting behaviors of ultra-thin polymer film on mica substrate
![Dewetting behaviors of ultra-thin polymer film on mica substrate](https://www.shimadzu.com/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000073uh-img/qn504200000073uy.jpg)
This height-image exhibits the dewetting pattern of ultra-thin polymer film on mica substrate. And the interaction between the polymer and the substrate surface can be evaluated by measuring the contact angle.
(Data provided by Prof. Xu-Ming Xie, Department of Chemical Engineering, Tsinghua University, China)